Hardness Testing

SEM- image, microhardness identation in  a structure phase of ADI-cast alloy
SEM- image, microhardness identation in a structure phase of ADI-cast alloy

The determination of the material hardness of steels, light metals, synthetics, elastomers and ceramics is performed with mobile and stationary systems. We determine case hardening, core hardening and hardness profiles according to customer specifications and/or current standards (CHD, RHT, NHT, DS). Macrohardness and microhardness tests are made on samples and components applying different loads from 0.01 to 250 kg/kp. 

  • Brinell
  • Vickers
  • Rockwell
  • Leeb
  • Shear force
  • Shore A and D
  • IRHD method M
  • Erichsen hardness test rod